Fibreglass Shingle

Also known as fiberglass shingle · glass-mat shingle · glass-fibre shingle

An asphalt shingle built on a glass-fibre mat; the dominant form of asphalt shingle sold today.

1 min read3 sourcesNorth AmericaGlobal
Cite this entry"Fibreglass Shingle." roof.wiki. https://roof.wiki/fiberglass-shingle/ (accessed 2026-11-02).
Mat
Glass-fibre, resin-bonded
Area weight
About 1.8-2.3 lb/sq ft (8.8-11.2 kg/m²)
Fire rating
Up to Class A
US standard
ASTM D3462 (min. 1,700 g tear strength)

Quick answers

What is Fibreglass Shingle?
An asphalt shingle built on a glass-fibre mat; the dominant form of asphalt shingle sold today.
What fire rating does Fibreglass Shingle have?
Up to Class A
Which standards apply to Fibreglass Shingle?
ASTM D3462 (min. 1,700 g tear strength)

A fibreglass shingle (US spelling: fiberglass) is an asphalt shingle whose reinforcing core is a non-woven mat of glass fibres bonded with resin, usually urea-formaldehyde. The mat is coated with asphalt that contains powdered mineral filler, then surfaced with granules. Almost all asphalt shingles made today are of this type.

Eave · starter course first Courses go on fromthe eave up. Each onecovers the nails below;joints are offset.
How shingles are laid

History

Glass-fibre mats were introduced in 1960 with limited success at first. Improvements in mat and coating technology followed, and by about 1982 fibreglass shingles had overtaken organic-felt shingles in the United States. By 2011 organic shingles had disappeared from North American production.

Properties

  • Lighter: the glass mat needs less asphalt, so area weights are typically about 1.8-2.3 lb/sq ft (8.8-11.2 kg/m²).
  • Fire resistance: glass-mat shingles can achieve a Class A fire rating under ASTM E108 / UL 790, the highest class.
  • Moisture: the glass mat does not absorb water, so the shingle is less prone to rot-related curling.
  • Brittleness: early products could crack in cold weather or during handling; polymer-modified asphalts were later introduced to improve flexibility.

Standards

In the United States, ASTM D3462 is the main product standard for glass-felt asphalt shingles surfaced with mineral granules, and the International Building Code requires asphalt shingles to comply with it. The standard sets a minimum Elmendorf tear strength of 1,700 g. In Canada, CSA standards apply, and in Europe glass-fibre bitumen shingles are covered by the European harmonised standard for bitumen shingles.

Quality

Weight alone is no longer a reliable sign of quality. Industry commentary notes that mat strength and coating quality vary between products, and a moderate-weight shingle with a strong mat can outperform a heavier one with a weak mat.

On the timeline

  1. 1700The standard sets a minimum Elmendorf tear strength of 1,700 g.
  2. 1960Glass-fibre mats were introduced in 1960 with limited success at first.
  3. c. 1982Improvements in mat and coating technology followed, and by about 1982 fibreglass shingles had overtaken organic-felt shingles in the United States.
See the full roofing timeline →

Sources

Reviewed 2 November 2026 · 3 sources · Editorial policy · Plain-text version · Suggest a correction

  1. Asphalt shingleWikipedia · en.wikipedia.org
  2. Q&A: Fiberglass vs. Organic ShinglesJournal of Light Construction · jlconline.com

From the community

Know this topic first-hand? Share a photo you took, a correction with a source, or local knowledge. Every contribution is reviewed before it appears.

Contribute to Fibreglass Shingle

Sign in with your email. We'll send a one-time link; no password needed.